I do need 2 top layers when printing at 0.2mm.

Everything here is printed with eSun PETG.

I've been prototyping a few things, so I've been interesting in tuning the settings so in the end I'd get something that uses least amount of plastic while the part doesn't fall apart immediately.

I should probably use PLA for this, but PETG would be final material, and gray color that I only have in PETG looks good on the photos.